Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.1 kV/mm | 333 kV/in | Short Time; ASTM D149 |
Plenco 1500 Polyester, Granular, Transfer Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Dielectric Strength | 13.1 kV/mm | 333 kV/in | Short Time; ASTM D149 |
Plenco 4504 Phenolic, Granular, Compression Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |
|||
Dielectric Strength | 13.1 kV/mm | 334 kV/in | ASTM D149 |
3M Scotchcast™ 2136 Potting Kit The 3M Scotchcast Potting Kit 2136 is designed to provide protection against corrosion and possible deteriorating effects of fresh swimming pool or fountain water and sunlight by reliably encapsulat.. |
|||
Dielectric Strength | 13.1 kV/mm | 333 kV/in | BS 903 |
Sorbothane Polyurethane Damping Material, 70 Durometer Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the mat.. |