Physical Properties Metric English Comments
Viscosity 1694 cP
1694 cP
Polyol [Part B]; 3M Method TM-173
3M Scotchcast™ 2136 Potting Kit
The 3M Scotchcast Potting Kit 2136 is designed to provide protection against corrosion and possible deteriorating effects of fresh swimming pool or fountain water and sunlight by reliably encapsulat..