ATI Allegheny Ludlum AL 440C™ Martensitic Stainless Steel, UNS S44004

Category Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum AL 440C™ Martensitic Stainless Steel, UNS S44004.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hardenable to high hardness levels for wear resistance applications and corrosion resistance above carbon steel. Typical uses in bearing, valve parts, cutlery and industrial knives.Information provided by Allegheny Ludlum
Component Elements Properties Metric English Comments
Carbon, C 1.0 %
1.0 %
Chromium, Cr 16.5 %
16.5 %
Iron, Fe 82.5 %
82.5 %
as balance