Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM 792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
10 seconds; ASTM D2240
Tensile Strength, Yield 4.83 MPa
700 psi
Elastic; ASTM D412
Elongation at Break 700 %
700 %
Elastic; ASTM D412
Tear Strength 22.8 kN/m
130 pli
ASTM D624
Thermal Properties Metric English Comments
Flame Spread 25 mm/min
0.98 in/min
FM VSS-302
Processing Properties Metric English Comments
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 227 °C
440 °F
Nozzle Temperature 235 °C
455 °F
Mold Temperature 51.7 °C
125 °F