3M Scotch-Weld™ PR100 Plastic and Rubber Instant Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ PR100 Plastic and Rubber Instant Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates or in combination with metal or composite substrates. Superior performance is achieved on materials such as heavily plasticized PVC, EPDM, ABS, Nylon, Santoprene® and Viton®. PR100 (formerly SB04 or SB14) is a general purpose, low viscosity bonder for rubber or plastic surfaces. It has been tested and passed the requirements of Commercial Item Description A-A 3097, Type II, Class 3 (formerly MIL-A-46050C).Information provided by 3M
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Viscosity 8.0 - 120 cP
8.0 - 120 cP
ISO 3104/3105
Mechanical Properties Metric English Comments
Shear Strength 21.4 MPa
3100 psi
cured, grit-blasted steel; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.167 - 0.500 min
0.00278 - 0.00833 hour
Time to Handling Strength
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid
Users viewing this material also viewed the following: