Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 8.0 cP | 8.0 cP | |
Lord Adhesives AP-134 Reactive Polymer Primer or Adhesive for Polar Substrates Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Viscosity | 8.0 cP @Temperature 25.0 °C |
8.0 cP @Temperature 77.0 °F |
|
LyondellBasell TPNB Tripropylene glycol normal butyl ether Information provided by Lyondell. |
|||
Viscosity | 8.0 - 25 cP | 8.0 - 25 cP | As Supplied |
Heraeus Cleviosâ„¢ PH 500 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PH 500 is an antistatic material based on PEDO.. |
|||
Viscosity | 8.0 - 10 cP @Temperature 20.0 °C |
8.0 - 10 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 51-08 Polyvinyl Alcohol Partially Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 8.0 cP | 8.0 cP | |
Dow Corning SYL-OFF® 7210 RELEASE MODIFIER Syl-Off® 7210 Release Modifier is a 60% active solids, pre-catalysed, release modifier. General purpose release modifier recommeded for use with Syl-Off® Solvent based, platinum catalysed release .. |
|||
Viscosity | 8.0 cP @Temperature 15.5 °C |
8.0 cP @Temperature 59.9 °F |
|
Dow Hydroxyethyl Acrylate Hydroxethyl Acrylate for high performance coatings. (Clear, colorless liquid)Information provided by Dow |
|||
Viscosity | <= 8.0 cP | <= 8.0 cP | |
3M Scotchgard™ 18 Low Maintenance Floor Finish Scotchgard Low Maintenance 18 Floor Finish, a high quality water-based co-polymer emulsion, is an economical finish designed to provide exceptional performance for low traffic areas and low frequenc.. |
|||
Viscosity | <= 8.0 cP | <= 8.0 cP | |
3M Scotchgard™ 25 Low Maintenance Floor Finish Scotchgard Low Maintenance 25 Floor Finish, a high quality water-based co-polymer emulsion, is designed to provide superior performance compared to traditional acrylic floor finishes for low frequen.. |
|||
Viscosity | <= 8.0 cP | <= 8.0 cP | |
3M Scotchgard™ Resilient Floor Protector Scotchgard Resilient Floor Protector is a high performance protective floor coating for vinyl tile and vinyl sheet flooring that utilizes multiple polymer technologies to produce a hard surface that.. |
|||
Viscosity | 8.0 - 120 cP | 8.0 - 120 cP | ISO 3104/3105 |
3M Scotch-Weld™ PR100 Plastic and Rubber Instant Adhesive 3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates .. |