Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 315A (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 362CPT (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 500R Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 717AR (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 723MS (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 732M (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Cured |
Parker Chomerics Tecknit® 73-00081 Electrically Conductive Acrylic and Polyurethane Paint Description: TECKNIT manufactures a highly conductive acrylic and polyurethane paints filled with silver. These coatings provide a cost effective method for shielding and grounding plastic enclosure.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
Resin Technology Group UV-406 Millennium™ UV Curable Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 706CS (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 706D-UV (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 902B (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
Permabond 931 Cyanoacrylate PERMABOND 931 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
Permabond 932 Cyanoacrylate PERMABOND 932 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
Resin Technology Group UV-403 Millennium™ UV Curable Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Retraction Temperature, TR10; ASTM D1329 |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with TP-95 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Continuous useful temperature. |
Momentive Performance Materials RTV21 Pink General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Continuous useful temperature. |
Momentive Performance Materials RTV31 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
Momentive Performance Materials RTV8262 Silicone Rubber Compounds for Potting, Encapsulating and Sealing RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M 431 Premium Performance Aluminum Foil Tape Conformable aluminum tape. UL 723 ClassifiedInformation provided by 3M |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-275 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-275 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-350 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-350 Class C-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-360 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-360 Class B are fast cure, intermediate density two-component, manganese dioxide cure, polysulfide fuel tank and fuselage sealant. 3M AC-360 Class B Sealants have outstanding.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ FLX300 Flexible Instant Adhesive 3M™ Scotch-Weld™ Flexible Instant Adhesive FLX (formerly PR851) is formulated for extended resistance to impact, vibration, stress, peel, and humidity applications. It is faster curing than 3M™ S.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ LO5 Low Odor Instant Adhesive 3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ HP45 Pipe Sealant Anaerobic Adhesives 3M™ Scotch-Weld™ Pipe Sealant Anaerobic Adhesives are one-component anaerobic sealants that cure and seal hydraulic and pneumatic pipes and fittings to withstand high temperatures and pressures. H.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ PR Gel Plastic and Rubber Instant Adhesive 3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates .. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Continuous |
3M Scotch-Weld™ RT300B Rubber-Toughened Instant Adhesive 3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bon.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | AMS-S83318 |
3M AC-250 B-1/6 Aerospace Sealant 3M Aerospace Sealant AC-250 B-1/6 is a two-part, polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a thixotropic paste and can be read.. |