Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 7906 Screen Printable Sheet Vinyl Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7906 Screen Printable Sheet Vinyl Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These materials utilize 3M™ Adhesive 300, which has excellent quick tack and also bonds well to a variety of surfaces including LSE plastics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Adhesive
86.4 microns
3.40 mil
Facestock
170 microns
6.70 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.0438 kN/m
0.250 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.07669 kN/m
0.4375 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.1424 kN/m
0.8125 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.153 kN/m
0.875 pli
Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.1972 kN/m
1.125 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.27391 kN/m
1.5625 pli
LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.2849 kN/m
1.625 pli
LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.2849 kN/m
1.625 pli
HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.29582 kN/m
1.6875 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.29582 kN/m
1.6875 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.31773 kN/m
1.8125 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.31773 kN/m
1.8125 pli
Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.3287 kN/m
1.875 pli
HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.351 kN/m
2.00 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.36156 kN/m
2.0625 pli
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.3725 kN/m
2.125 pli
HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.394 kN/m
2.25 pli
LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.394 kN/m
2.25 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.40538 kN/m
2.3125 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.40538 kN/m
2.3125 pli
Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.40538 kN/m
2.3125 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.40538 kN/m
2.3125 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.4163 kN/m
2.375 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.42729 kN/m
2.4375 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.438 kN/m
2.50 pli
Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.438 kN/m
2.50 pli
LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.4602 kN/m
2.625 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.4602 kN/m
2.625 pli
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.47112 kN/m
2.6875 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.47112 kN/m
2.6875 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.47112 kN/m
2.6875 pli
Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.5040 kN/m
2.875 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.526 kN/m
3.00 pli
Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.60259 kN/m
3.4375 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.60259 kN/m
3.4375 pli
Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.6355 kN/m
3.625 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.657 kN/m
3.75 pli
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.657 kN/m
3.75 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.657 kN/m
3.75 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.657 kN/m
3.75 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.701 kN/m
4.00 pli
Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.7231 kN/m
4.125 pli
Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.73407 kN/m
4.1875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.73407 kN/m
4.1875 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.745 kN/m
4.25 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.745 kN/m
4.25 pli
Glass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.8108 kN/m
4.625 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.82172 kN/m
4.6875 pli
Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
5.00 °C
41.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 300 Acrylic
Liner 90# Polyctd.
Copyright © lookpolymers.com All Rights Reserved