Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.82172 kN/m | 4.6875 pli | to Steel; ASTM D3330 |
3M 1026 Adhesive Transfer Tape 3M™ Adhesive Transfer Tape 1026 is a 300 high strength acrylic adhesive on a 4 mil liner. Adhesive transfer tape in a pre-cut, tape strip on a pad.Features:5.0 mil adhesive transfer tape on a pad. .. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9671 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Stainless Steel, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330 |
3M 9671LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9673 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | to Steel, Initial, 12 in/min |
3M 9740 Double Coated Tape 3M™ Double Coated Tape 9740 is a 3.5 mil double coated tape utilizing a 0.5 mil (12 microns) polyester film coated on both sides with 1.5 mils (38 microns) of a high shear acrylic adhesive system. .. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 8651 Strapping Tape Scotch® Strapping Tape is a high-performance, transparent packaging tape reinforced along its length with continuous polypropylene monofilaments, which give the tape high tensile strength. The poly.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 8916 Filament Tape Scotch® Filament Tape 8916 is a high-performance transparent tape reinforced with continuous high strength glass filaments which is designed to hold appliance parts together during manufacture and .. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Adhesion to Steel; ASTM D3330 |
3M 5430 Squeak Reduction Tape 3M™ Squeak Reduction Tapes are a film tape for the automotive industry to help control squeaks and rattles due to vibration or wear of metal and plastic materials.Information provided by 3M |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | 90° Peel, PET/Polycarbonate, 72 hrs at 70°C; ASTM D3330 |
3M 7953MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Adhesion to Anodized Aluminum, after Thermal Cycling; ASTM D3330 |
3M 8777 Sealing Tape 3M™ Sealing Tape 8887 is a self-adhered, waterproof membrane designed for sealing on difficult to stick to surfaces. This product has a unique acrylic pressure sensitive adhesive that aggressively .. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Adhesion to Steel; ASTM D3330 |
3M 9324 Squeak Reduction Tape 3M™ Squeak Reduction Tapes are a film tape for the automotive industry to help control squeaks and rattles due to vibration or wear of metal and plastic materials.Information provided by 3M |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 8626 Tear Tape Scotch® Tear Tape 8624 is a designed for use as the easy-opening device on paperboard and light- to medium-weight corrugated fiberboard packaging materials. Typical easy-opening applications for Sc.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 8898 Strapping Tape Scotch® Strapping Tape 8896 is a ge3neral-purpose tape with a tensilized polypropylene film backing and pressure-sensitive adhesive. The tape is designed for a wide variety of industrial and packag.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | 90° Peel, PET/Aluminum, 72 hrs at RT; ASTM D3330 |
3M 7997MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | 90° Peel, PET/Aluminum, 72 hrs at RT; ASTM D3330 |
3M 9056MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.82172 kN/m | 4.6875 pli | HDPE, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330 |
3M 9629PC Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |