Thermal Properties Metric English Comments
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M 7331/7860 Thermal Transfer Polyester Label Material
3M™ Thermal Transfer Polyester Label Materials are durable polyester stocks that offer high abrasion and chemical resistance. These materials utilize 3M™ Adhesive 300, which has excellent quick ta..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FM037 Indoor UL Recognized Clear Polyester Label Products
on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FM03R2 Indoor UL Recognized Clear Polyester Label Products
on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FM059 Indoor UL Recognized Brite Silver Polyester Label Products
3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FM06P Indoor UL Recognized Brite Silver Polyester Label Products
3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FM071 Indoor UL Recognized Clear Polyester Overlaminate Label Product
3M™ Indoor UL Recognized Matte Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester ov..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FM122R Indoor UL Recognized White Polyester Label Products
3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FM691 Indoor UL Recognized Computer Imprintable Clear Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Service
3M FP017102 White Polyester Label Products
3M™ White Polypropylene Label Products FP017102 and FP026508 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general purpose permane..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FP01G Clear Polypropylene Label Products
3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Service
3M FP024900 White Polypropylene Label Products
3M™ White Polypropylene Label Products are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FP531 Clear Polypropylene Label Products
3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FV06B Semi-Rigid White Vinyl Label Product
3M™ Semi-Rigid White Vinyl Label Products are white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clarity general..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FV1222 Removable Vinyl Label Products
3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FVT40 Tire Label Product
3M™ Tire Label Products utilize a flexible and conformable white vinyl labelstock that offers durability, moisture resistance, and dimensional stability. 3M™ Adhesive G1120, a rubber-based aggress..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Service
3M OFM0103 Outdoor UL Recognized Polyester Overlaminate Label Products
3M™ Outdoor UL Recognized Polyester Overlaminate Label Products are durable high performance clear materials that offer excellent thermal stability, abrasion and moisture resistance. These polyeste..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M OFM0402 Outdoor UL Recognized White Polyester Label Product
3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ ..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M OFM1603 Outdoor UL Recognized Clear Polyester Label Product
3M™ Outdoor UL Recognized Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ ..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M SJ5201 Protective Product, Die Cut Shapes
3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M 7222/7865 Thermal Transfer Polyester Label Material
3M™ Thermal Transfer Polyester Label Materials are durable polyester stocks that offer high abrasion and chemical resistance. These materials utilize 3M™ Adhesive 300, which has excellent quick ta..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M 7925 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FL01100N Lexan Label Product
3M™ Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P1212, which is a high ..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Service
3M FM482 Clear Polyester Label Product
3M™ Clear Polyester Label Product FM482 is a durable, high performance material that offers thermal stability and moisture resistance. This polyester label product utilizes 3M™ Adhesive P1110, whi..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FMV01402 Triangle Void Polyester Label Products
3M™ Triangle Void Polyester Label Products FMV01202 and FMV01402 are a tamper-indicating stock designed to provide a triangle pattern in the facestock when removal is attempted. These label product..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FP010609 Matte White Polypropylene Label Product
3M™ Matte White Polypropylene Label Products FP010602, FP010609 and FP017802 are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FP029202 White Polypropylene Label Product
3M™ White Polypropylene Label Products FP02750N and FP029202 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1480 which is a high performance tackifi..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M FV032 Indoor UL Recognized White Vinyl Label Products
3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M OFM0403 Outdoor UL Recognized White Polyester Label Product
3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ ..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M OFM0802 Outdoor UL Recognized Brite Silver Polyester Label Products
3M™ Outdoor UL Recognized Brite Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize..
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Application
3M OFL020N Outdoor UL Recognized Lexan Label Products
3M™ Outdoor UL Recognized Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P..