Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.153 kN/m | 0.875 pli | Adhesion to Steel; ASTM D3330 |
3M 2187 Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 2187 has a high-tack adhesive system to help provide temporary protection of many metals, plastics and painted metal panels with minimum adhesion build up and clea.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | LD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7000FL Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | LD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7000FL Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | LD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7000FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | HD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7002 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | HD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7002FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | Adhesion to Neoprene; ASTM D1000 |
3M Scotch® 31 Heavy Duty Mining Tape Scotch® Heavy Duty Mining Tape 31 has a tough, abrasion-resistant backing for jacket repair on mining cables. Due to extremely abrasive environment, the original jacket on the cable gets damaged of.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | Adhesion to Steel; ASTM D3330 |
3M 2A87 Co-Extruded Multi-Polymer Protect Tapes 3M™ Co-Extruded Multi-Polymer Protective Tapes have a high-tack adhesive system to help provide temporary protection for a variety of surface protection applications.Information provided by 3M |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7920 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive .. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7776 Polypropylene Label Material 3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.153 kN/m | 0.875 pli | Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |