Material Notes:
Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 500 system.All information provided by 3D Systems.
Physical Properties Metric English Comments
Density 1.10 g/cc

@Temperature 25.0 °C
0.0397 lb/in³

@Temperature 77.0 °F
Liquid
Viscosity 485 cP

@Temperature 30.0 °C
485 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
ASTM D2240
Tensile Strength, Yield 55.0 - 57.0 MPa
7980 - 8270 psi
ASTM D638
Elongation at Break 5.8 - 7.8 %
5.8 - 7.8 %
ASTM D638
Tensile Modulus 2.701 - 2.978 GPa
391.7 - 431.9 ksi
ASTM D638
Flexural Strength 80.0 - 83.0 MPa
11600 - 12000 psi
ASTM D790
Flexural Modulus 2.147 - 2.286 GPa
311.4 - 331.6 ksi
ASTM D790
Izod Impact, Notched 0.202 - 0.213 J/cm
0.378 - 0.399 ft-lb/in
ASTM D256
Penetration 4.4
4.4
mils
Thermal Properties Metric English Comments
CTE, linear 62.0 µm/m-°C
34.4 µin/in-°F
T<Tg; ASTM E831-93
108 µm/m-°C
60.0 µin/in-°F
T>Tg; ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 57.0 °C
135 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C
124 °F
ASTM D648
Glass Transition Temp, Tg 40.0 °C
104 °F
DMA, E"
Descriptive Properties Value Comments
Appearance Clear amber
Critical Exposure (mJ/cm²) 7.4
Tested Build Styles EXACT™, QuickCast