Polymer Property : Tensile Strength, Yield = 57.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.14 - 57.0 MPa
600 - 8270 psi
Average value: 19.9 MPa Grade Count:13
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
Tensile Strength, Yield 53.0 - 57.0 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
7690 - 8270 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Tensile Strength, Yield 53.0 - 57.0 MPa

@Thickness 2.00 mm
7690 - 8270 psi

@Thickness 0.0787 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: MembranesAddition..
Tensile Strength, Yield 53.0 - 57.0 MPa

@Thickness 2.00 mm
7690 - 8270 psi

@Thickness 0.0787 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran..
Tensile Strength, Yield 55.0 - 57.0 MPa
7980 - 8270 psi
ASTM D638
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 500 System
Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 500 system.All information provided by 3D Systems.
Tensile Strength, Yield 53.0 - 57.0 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
7690 - 8270 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Tensile Strength, Yield 53.0 - 57.0 MPa
7690 - 8270 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer  (discontinued **)
Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
Tensile Strength, Yield 53.0 - 57.0 MPa
7690 - 8270 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer  (discontinued **)
Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO..
Tensile Strength, Yield 53.0 - 57.0 MPa
7690 - 8270 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer  (discontinued **)
Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
Tensile Strength, Yield 53.0 - 57.0 MPa
7690 - 8270 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer  (discontinued **)
Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c..