Material Notes:
Description: Polymer to be used in acidic hard surface cleaners and delivering the following benefits through surface modification: spot free, easy cleaning, water sheeting and fast drying. pH 2 to 6.Identification: Aqueous solution of an acrylic based polymerUse level: 0.5 – 1% as isNotes: Polymer soluble in water in all proportions, compatible with common non ionic, cationic and amphoteric surfactants. Not compatible with anionic surfactants. Compatibility with thickeners to be checked.Available in: Asia Pacific, Europe, Latin America and North America Applications: Mirapol SURF-S 110 is EPA approved as an inert ingredient (co-formulant) in non-food contact, hard-surface sanitizers. Use levels of this product are limited to 4% in the formulation. Recommended for formulations from pH 1 to 12. Polymer to be used in hard surface cleaners and delivering the following benefits through surface modification: spot free, easy cleaning, water sheeting and fast drying.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Solids Content 19 - 23 %

@Temperature 105 °C,
Time 7200 sec
19 - 23 %

@Temperature 221 °F,
Time 2.00 hour
4 grams in 40g sand; 540MC3C30
pH 3.5 - 4.5
3.5 - 4.5
540MA3C1E
Viscosity <= 200 cP
<= 200 cP
LV#1, 30 rpm; 540MO3C16
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear to slightly hazy liquid
540MA3C1F
Composition Gram Negative
<10 cfu/ml, Z128
Staphylococcus aureus
<10 cfu/ml, Z128
Total Plate Count
<500 cfu/ml, Z128
Yeast & Mold
<500 cfu/ml, Z128
Preservative 1,2-benzisothiazol-3(2H)-one
0.00015
2-methyl-2H-isothiazol-3-one
0.00015
3-Iodo-2-propynyl butylcarbamate
9E-05