Polymer Property : Flexural Strength = 12000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 68.9 - 82.7 MPa
10000 - 12000 psi
ASTM D790
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Flexural Strength 68.9 - 82.7 MPa
10000 - 12000 psi
ASTM D790
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Flexural Strength 80.0 - 83.0 MPa
11600 - 12000 psi
ASTM D790
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 500 System
Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 500 system.All information provided by 3D Systems.
Flexural Strength 68.9 - 82.7 MPa
10000 - 12000 psi
Bulk Molding Compounds BMC 501E Mineral Filled, Glass Reinforced Polyester
BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame..
Flexural Strength 68.9 - 82.7 MPa
10000 - 12000 psi
Bulk Molding Compounds BMC 901 Encapsulating Grade Molding Compound
BMC 901 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an..
Flexural Strength 62.1 - 82.7 MPa
9000 - 12000 psi
Bulk Molding Compounds BMC 902 Thermoset Polyester, Soft Flow Encapsulation Grade
BMC 902 is a medium strength, high flow molding compound that meets Ford Specification ESFM3D114- A. BMC 902 has excellent electrical properties and creep resistance. It can be pigmented in a wide r..
Flexural Strength 62.1 - 82.7 MPa
9000 - 12000 psi
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, ..
Flexural Strength 68.9 - 82.7 MPa
10000 - 12000 psi
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade
BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B..
Flexural Strength 68.9 - 82.7 MPa
10000 - 12000 psi
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade
BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an..