Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 - 1.00e+9 ohm-cm
1.00e+6 - 1.00e+9 ohm-cm
ASTM D257
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific)
Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD.
Volume Resistivity 1.00e+6 - 1.00e+9 ohm-cm
1.00e+6 - 1.00e+9 ohm-cm
ASTM D257
Techmer ES Statiblend® PA6/6 02013
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedUL File Number: E157318TPCI# 1039101Informati..
Volume Resistivity 1.00e+6 - 1.00e+9 ohm-cm
1.00e+6 - 1.00e+9 ohm-cm
ASTM D257
Techmer ES Statiblend® PBT 03003
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass FiberFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Composites, Inc.
Volume Resistivity 1.00e+6 - 1.00e+9 ohm-cm
1.00e+6 - 1.00e+9 ohm-cm
ASTM D257
Techmer ES Statiblend® PBT GF10 SS5 MB
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: AntistaticFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Comp..
Volume Resistivity 1.00e+7 - 1.00e+9 ohm-cm
1.00e+7 - 1.00e+9 ohm-cm
ASTM D257
Techmer ES Statiblend® POM CO AS
Availability: North AmericaForms: PelletsAdditive: AntistaticFeature: Antistatic and ConductiveTPCI# 60000114Information provided by TP Composites, Inc.
Volume Resistivity 1.00e+7 - 1.00e+9 ohm-cm
1.00e+7 - 1.00e+9 ohm-cm
ASTM D257
Techmer ES Statiblend® POM CO AS BK
Availability: North AmericaForms: PelletsAdditive: AntistaticFeature: Antistatic and ConductiveAppearance: BlackInformation provided by TP Composites, Inc.
Volume Resistivity 1.00e+6 - 1.00e+9 ohm-cm
1.00e+6 - 1.00e+9 ohm-cm
Dry; ASTM D257
Westlake Plastics Propylux® SD-X7 Polypropylene (static dissipative)
Low carbon black content (1-2%) reduces contamination problems from sloughing - clean room compatible. Also feature low leachable ion levels and low outgassing.Information provided by Westlake Plas..
Volume Resistivity 1.00e+8 - 1.00e+9 ohm-cm
1.00e+8 - 1.00e+9 ohm-cm
Practical Use (Water Absorption 3.5%); ASTM-D257
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Volume Resistivity 1.00e+8 - 1.00e+9 ohm-cm
1.00e+8 - 1.00e+9 ohm-cm
Practical Use (Water Absorption 3.0%); ASTM-D257
Toyobo GLAMIDE® T-808-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Volume Resistivity 1.00e+8 - 1.00e+9 ohm-cm
1.00e+8 - 1.00e+9 ohm-cm
Practical Use (Water Absorption 1.8%); ASTM-D257
Toyobo GLAMIDE® T-422VOR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Volume Resistivity 1.00e+8 - 1.00e+9 ohm-cm
1.00e+8 - 1.00e+9 ohm-cm
Practical Use (Water Absorption 3.5%); ASTM-D257
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..