Electrical Properties Metric English Comments
Volume Resistivity <= 1.00e+6 ohm-cm
<= 1.00e+6 ohm-cm
Teil 30; IEC 600093 / VDE 0303
Okulen® 500 PE-HMW, AST
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
Volume Resistivity <= 1.00e+6 ohm-cm
<= 1.00e+6 ohm-cm
ISO D-257
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound
PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS..
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
Parker Chomerics CHO-MUTE 9020 RF Absorber
Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 30 MHz to 12 GHz. CHO-MUTE 9020 incorporates a high tech silicone..
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
VDE 0303
GEHR Plastics PE-UHMW-ELS Polyethylene  (discontinued **)
Polyethylene offers resistance to almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature of HDPE is from -58 °F to +1..
Volume Resistivity 1e+05 - 1.00e+6 ohm-cm
1e+05 - 1.00e+6 ohm-cm
ASTM D257
LG Chemical LUCON PO-3000 Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
ASTM D257
Haysite H208 Polyester, Magnetic Permeable
Grade H208 has high magnetic permeability and excellent retention of properties after heat aging at elevated temperatures. This unique combination of properties allows Grade H208 to be used in vari..
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
ASTM D257
Techmer ES HiFill® PEEK CF40 HF 40% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc.
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
ASTM D257
Techmer ES HiFill® PVDF CF15-M BK 15% Milled Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Carbon Fiber, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
ASTM D257
Borealis FR4837 Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires
FR4837 is a chemically crosslinkable Non-halogen flame retardant Polyethylene compound for Primary Automotive and Appliance Wire. Applications: FR4837 is intended for use as a 125º C rated primary..
Volume Resistivity 1e+05 - 1.00e+6 ohm-cm
1e+05 - 1.00e+6 ohm-cm
UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE.
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
IEC 60250
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable
LE4201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications LE4201R is intended for insulation of XLPE power cables with rated voltages up..
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
IEC 60093
Borealis SuperCOPO™ LE4205R Polyethylene Insulation Compound, Crosslinkable
SuperCOPO™ LE4205R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: SuperCOPO™ LE4205R is intended for insulation of XLPE power cabl..
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
IEC 60093
Borealis Supercure™ LC8205R Polyethylene Insulation Compound, Crosslinkable
Supercure™ LC8205R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Supercure™ LC8205R is intended for insulation of XLPE power cabl..
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
IEC 60093
Borealis Visico™/Visico™ LE4421M/LE4431M Polyethylene
Visico™ LE4421M / Visico™ LE4431M is a two-part silane crosslinkable insulation system, specially designed for insulation applications. Applications: Visico™ LE4421M / Visico™ LE4431M is intend..
Volume Resistivity 1.00e+6 - 1.00e+9 ohm-cm
1.00e+6 - 1.00e+9 ohm-cm
Dry; ASTM D257
Westlake Plastics Propylux® SD-X7 Polypropylene (static dissipative)
Low carbon black content (1-2%) reduces contamination problems from sloughing - clean room compatible. Also feature low leachable ion levels and low outgassing.Information provided by Westlake Plas..
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
IEC 60093
Borealis Casico™ FR4820 Natural Low Smoke Zero Halogen Flame Retardant Insulation Compound for Building Energy Cables
Casico™ FR4820 is a thermoplastic, low smoke zero halogen (LSZH) flame retardant, UV stabilized, natural insulation compound combining with excellent extrusion properties. It is based on the novel..
Volume Resistivity 1.00e+6 - 1.00e+7 ohm-cm
1.00e+6 - 1.00e+7 ohm-cm
CoorsTek StatSafe™ ADC Static Dissipative Alumina
Specialized StatSafe™ ESD-safe alumina combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffnes..
Volume Resistivity 1.00e+6 - 1.00e+7 ohm-cm
1.00e+6 - 1.00e+7 ohm-cm
CoorsTek StatSafe™ ZDC-W Static Dissipative Zirconia
Specialized StatSafe™ ESD-safe zirconia combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffne..
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
Cotronics Duralco™ 132 500°F (260°C) Aluminum Filled Epoxy
Aluminum filled epoxy that cures at room temperature to form machinable, thermally conductive bond lines. High heat transfer. Can be supplied as a “non-sag” putty.Applications: heat tacking, hea..
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
conditioned; IEC 60093
EMS-Grivory Grivory® LV-3 ESD PA12-GF30
Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where..
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
ASTM D257
Adamas Rixon 430 PEEK, 30% Carbon Fiber
Information provided by Adamas, HPM
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
Bulk, Initial; CEPS-0002
Parker Chomerics CHO-MUTE 9005 Microwave Absorber
Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon..
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
DC; IEC 60093
Borealis LE6025 Polyethylene Modified Jacketing Compound
LE6025 is a black low density copolymer modified polyethylene compound. It is characterized by excellent stress crack resistance and mechanical properties and low temperature performance in combinat..
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
IEC 60093
Borealis Visico™/Ambicat™ LE4421/LE4476 Polyethylene Compound, Crosslinkable
Visico™ LE4421 / Ambicat™ LE4476 is a silane crosslinkable natural compound designed for low voltage power cables up to 6kV. The base material Visico™ LE4421 in combination with the catalyst mas..
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
DC; IEC 60093
Borealis Borstar® LE8707 Black Bimodal LLDPE Jacketing Compound for Energy and Communication Cables
Borstar® LE8707 is a black linear low density (LLD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar® technology allows the manufa..