Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Statiblend® PBT 03003

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
Manufacturer Techmer ES
Trade Name Statiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® PBT 03003.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass FiberFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.080 %

@Time 86400 sec
0.080 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Thickness 3.17 mm
0.0090 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 49.6 MPa
7200 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm
0.900 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 8.01 J/cm

@Thickness 3.17 mm
15.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 108 °C
226 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 - 1.00e+9 ohm-cm
1.00e+6 - 1.00e+9 ohm-cm
ASTM D257
Surface Resistance 1.00e+6 - 1.00e+9 ohm
1.00e+6 - 1.00e+9 ohm
ASTM D257
Static Decay <= 2.0 sec
<= 2.0 sec
MIL PRF-81705D