Westlake Plastics Propylux® SD-X7 Polypropylene (static dissipative)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with Carbon Black Filler
Manufacturer Westlake Plastics
Trade Name Propylux® SD-X7
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Propylux® SD-X7 Polypropylene (static dissipative).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low carbon black content (1-2%) reduces contamination problems from sloughing - clean room compatible. Also feature low leachable ion levels and low outgassing.Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C
300 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 - 1.00e+9 ohm-cm
1.00e+6 - 1.00e+9 ohm-cm
Dry; ASTM D257
Surface Resistance 1.00e+6 - 1.00e+9 ohm
1.00e+6 - 1.00e+9 ohm
Dry; ASTM D257