Polymer Property : Dielectric Strength = 800 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 31.5 kV/mm

@Thickness 1.60 mm
800 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer
Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele..
Dielectric Strength 31.5 kV/mm

@Thickness 1.60 mm
800 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific)
Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele..
Dielectric Strength 31.5 kV/mm

@Thickness 1.60 mm
800 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele..
Dielectric Strength 31.5 kV/mm
800 kV/in
Short Time; 1/8 inch; ASTM D149
G-10 Fiberglass Epoxy Laminate Sheet
This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e..
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D419
Teknor Apex Telcar® TL-1522B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D419
Teknor Apex Telcar® TL-1654D Thermoplastic Elastomer
Notes: Non-halogenated; RoHS Compliant; MBDC: Green Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General ..
Dielectric Strength >= 31.5 kV/mm
>= 800 kV/in
At 40 mils; ASTM D149
Borealis Visico™ ME4425/LE4462 Scorch Retardant Silane Crosslinkable MDPE Track Resistant Cable Insulation
Visico ME4425/LE4462 is a combination of LE4425, a Medium Density Visico base resin and a masterbatch, LE4462, which contains catalyst, carbon black, UV stabilizers and antioxidants. The LE4462 mas..
Dielectric Strength 31.5 - 66.9 kV/mm
800 - 1700 kV/in
ASTM D149
Zeus PVDF Tubing
PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char..
Dielectric Strength 31.5 kV/mm
800 kV/in
Tra-Con Tra-Bond 789-3 Moisture Resistant Adhesive
TRA-BOND 789-3 one component, high strength toughened adhesive is designed for microelectronic applications, including substrate attach and package sealing, which require good moisture resistance. I..
Dielectric Strength 31.5 kV/mm
800 kV/in
Tra-Con Tra-Bond 789-3TN1 Moisture Resistant Adhesive
TRA-BOND 789-3TN1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistanc..
Dielectric Strength 31.5 kV/mm
800 kV/in
2.03 mm; ASTM D149
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D149
Arlon P29514R015 0.0165" (0.419 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassProduct Advatages:Flexibility: Silicone rubber resists damage due to vibration, frame movement under loa..
Dielectric Strength 31.5 kV/mm
800 kV/in
Arlon SQA-TMS-020
Arlon P31000A005 0.005" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and should not be us..
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D149
Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D149
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D149
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val..
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D295
3M Scotch® 2510 Varnished Cambric Tape
Scotch® Varnished Cambric Tapes are made from straight-cut woven cotton cambric fabric. The fabric is oil primed and coated with a high-grade yellow electrical insulating varnish. Varnished cambric..
Dielectric Strength 31.5 kV/mm
800 kV/in
Standard Conditioning; ASTM D4325
3M Scotch™ 23 Rubber Splicing Tape
Scotch® Rubber Splicing Tape 23 is a highly conformable, self-fusing EPR (Ethylene Propylene Rubber) based, high voltage splicing tape. It is a non-vulcanizing, shelf-stable tape with excellent ele..
Dielectric Strength 31.5 - 43.3 kV/mm
800 - 1100 kV/in
ASTM D149
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st..
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D149
Arlon R38095R011 0.011" (0.279 mm) Partially Cross Linked Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Partially Cross Linked Silicone RubberSubstrate: Style 1528 Fiberglass:Side 2: Partially Cross Linked Silicone Rubber Product Use: Electrical InsulationAppearance: Red si..
Dielectric Strength 31.5 kV/mm
800 kV/in
3M EPS-200 Tubing
3M EPS-200 is a 2:1 thin-wall tubing offering the advantages of integral adhesive-lined construction. The tubing is made from a flame-retardant, flexible polyolefin with a thing layer of special the..
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D295
3M Scotch® 2520 Varnished Cambric Tape
Scotch® Varnished Cambric Tapes are made from straight-cut woven cotton cambric fabric. The fabric is oil primed and coated with a high-grade yellow electrical insulating varnish. Varnished cambric..
Dielectric Strength 31.5 kV/mm
800 kV/in
3M VFP-876 Tubing
3M VFP-876 is the most flexible of the heat-shrinkable, polyolefin tubings. Rated at 135°C. VFP-876 Tubing has been engineered to offer a low shrink temperature of 100°C. This allows the tubing to..
Dielectric Strength 31.5 - 43.3 kV/mm
800 - 1100 kV/in
ASTM D149
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Dielectric Strength 31.5 kV/mm
800 kV/in
DAM; IEC 60243-1
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont ..
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D149
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D149
Arlon R37480X008 0.008" (0.203 mm) Uncured Silicone Rubber with Substrate: PTFE Coated Fiberglass Substrate
Description: Primerless Thermabond® electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substra..
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D149
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier
Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber..
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D149
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber
Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib..