Material Notes:
3M EPS-200 is a 2:1 thin-wall tubing offering the advantages of integral adhesive-lined construction. The tubing is made from a flame-retardant, flexible polyolefin with a thing layer of special thermoplastic adhesive. The heat-shrinkable outer wall is selectively cross-linked while maintaining the high flow and excellent adhesion of the inner sealant liner. When heated in excess of 121°C, EPS-200 rapidly shrinks to a skintight fit, forcing the melted adhesive lining to flow and cover the substrate. The adhesive forms a flexible bond with a wide variety of rubbers, plastics and metals. Upon cooling, the adhesive solidifies forming a permanent, non-drying, flexible and water resistant barrier. EPS-200 is rated for operation at -55°C to 110°C. Adhesive reflow will occur at temperatures above 80°C.Information provided by 3M
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.5 MPa
2100 psi
Elongation at Break 450 %
450 %
175 %

@Temperature 175 °C,
Time 1.21e+6 sec
175 %

@Temperature 347 °F,
Time 336 hour
Heat Aged
Peel Strength 1.75 kN/m
10.0 pli
Adhesion to PVC
2.63 kN/m
15.0 pli
Adhesion to Lead
5.26 kN/m
30.0 pli
Adhesion to Polyethylene
7.01 kN/m
40.0 pli
Adhesion to Aluminum
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
300 °C
572 °F
for short periods
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Strength 31.5 kV/mm
800 kV/in