Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiberglass Product Use: Electrically insulating electronic thermal interface material.Appearance: Gray, solid (elastomer) with polymer linersThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 2.80 g/cc
0.101 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 38.1 microns
1.50 mil
Liner
76.2 microns
3.00 mil
Carrier
356 microns
14.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
Silicone Property; ASTM D2240
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Tensile Strength, Yield 24.5 MPa

@Strain <=1.00 %
3550 psi

@Strain <=1.00 %
Silicone Property; ASTM E 831
Elongation at Break 125 %
125 %
Silicone Property; ASTM D412
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Thermal Properties Metric English Comments
CTE, linear 105 µm/m-°C

@Temperature 20.0 - 160 °C
58.3 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E 831
Specific Heat Capacity 0.820 J/g-°C

@Temperature 100 °C
0.196 BTU/lb-°F

@Temperature 212 °F
Silicone Property; Arlon SQA-TMS-052
Thermal Conductivity 2.09 W/m-K
14.5 BTU-in/hr-ft²-°F
Product Property; Arlon SQA-TMS-054
1.40 W/m-K

@Temperature 100 °C
9.72 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; Arlon SQA-TMS-022
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Minimum Service Temperature, Air -136 °C
-212 °F
Glass Transition Temp, Tg -118 °C
-180 °F
ASTM D3418
Flammability, UL94 V-0
V-0
Not Recognized
Electrical Properties Metric English Comments
Dielectric Constant 7.07

@Frequency 1.00e+6 Hz
7.07

@Frequency 1.00e+6 Hz
D<sub>k</sub>, Silicone Property; IPC TM 650 - 2.5.5.3
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D149
Dissipation Factor 0.000023

@Frequency 1.00e+6 Hz
0.000023

@Frequency 1.00e+6 Hz
D<sub>f</sub>, Silicone Property; IPC TM 650 - 2.5.5.3
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.0 - 27.0 °C
60.0 Month

@Temperature 69.8 - 80.6 °F
From date of manufacture
Descriptive Properties Value Comments
Color Gray
Plasticity 2.3 mm
Arlon SQA-TMS-005
Total Product Weight (g/m2) 996
Arlon SQA-TMS-025
Copyright © lookpolymers.com All Rights Reserved