Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Thermabond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInformation provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns
1.00 mil
Liner
76.2 microns
3.00 mil
Carrier
381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Outgassing - Total Mass Loss 0.50 %
0.50 %
Arlon SQA-TMS-045
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
Silicone Property; ASTM D2240
Tensile Strength 2.07 MPa
300 psi
Silicone Property; ASTM D412
Elongation at Break 28 %
28 %
Silicone Property; ASTM D412
Modulus of Elasticity 0.0328 GPa
4.75 ksi
ASTM E 831
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Shear Modulus 0.000448 GPa
0.0650 ksi
ASTM D 1002
Shear Strength 1.28 MPa
185 psi
Lap Shear Strength; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 39.0 µm/m-°C
21.7 µin/in-°F
Silicone Property; ASTM E 831
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
E 1461-01
Thermal Conductivity 1.50 W/m-K
10.4 BTU-in/hr-ft²-°F
Silicone Property; ASTM E 1530
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Glass Transition Temp, Tg -110 - -95.0 °C
-166 - -139 °F
Silicone Property; ASTM D3418
Electrical Properties Metric English Comments
Dielectric Constant 3.8
3.8
D<sub>k</sub>, Silicone Property; IPC TM 650-2.5.5.3
Dielectric Strength 31.5 kV/mm
800 kV/in
ASTM D149
Dissipation Factor 0.0028
0.0028
D<sub>f</sub>, Silicone Property; IPC TM 650-2.5.5.3
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 121 °C
0.250 hour

@Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 4.44 - 10.0 °C
6.00 Month

@Temperature 40.0 - 50.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color White
Total Product Weight (g/m2) 655
Arlon SQA-TMS-025