Zeus PVDF Tubing

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer Zeus
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeus PVDF Tubing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is characterized by low permeability, as well as strong abrasion and chemical resistance.
Physical Properties Metric English Comments
Density 1.76 - 1.88 g/cc
0.0636 - 0.0679 lb/in³
ASTM D792
Water Absorption 0.010 - 0.060 %
0.010 - 0.060 %
ASTM D257
Crystallinity 35 - 70 %
35 - 70 %
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 82
65 - 82
ASTM D2240
Tensile Strength, Ultimate 17.0 - 48.0 MPa
2470 - 6960 psi
ASTM D638
Elongation at Break 50 - 400 %
50 - 400 %
ASTM D638
Modulus of Elasticity >= 0.500 GPa
>= 72.5 ksi
ASTM D638
Flexural Modulus >= 1.30 GPa
>= 189 ksi
ASTM D790
Coefficient of Friction 0.14 - 0.23
0.14 - 0.23
Thermal Properties Metric English Comments
CTE, linear 90.0 - 144 µm/m-°C

@Temperature 20.0 °C
50.0 - 80.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.170 - 0.190 W/m-K
1.18 - 1.32 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 172 °C
342 °F
Maximum Service Temperature, Air 100 - 130 °C
212 - 266 °F
Glass Transition Temp, Tg -40.0 - -30.0 °C
-40.0 - -22.0 °F
Decomposition Temperature 375 - 400 °C
707 - 752 °F
ASTM E1131
Oxygen Index 44 - 80 %
44 - 80 %
ASTM D2863
Optical Properties Metric English Comments
Refractive Index 1.42
1.42
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
ASTM D257
Dielectric Constant 7.0

@Frequency 1.00e+6 Hz
7.0

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 31.5 - 66.9 kV/mm
800 - 1700 kV/in
ASTM D149
Descriptive Properties Value Comments
Radiation Resistance (MRad) 1000