Material Notes:
Scotch® Rubber Splicing Tape 23 is a highly conformable, self-fusing EPR (Ethylene Propylene Rubber) based, high voltage splicing tape. It is a non-vulcanizing, shelf-stable tape with excellent electrical properties. Scotch® Tape 23 can be used as an insulation for low-voltage application as well as an insulation for splices up to 69,000 volts.Information provided by 3M
Physical Properties Metric English Comments
Thickness 762 microns
30.0 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.064 MPa
154.3 psi
ASTM D4325
Elongation at Break 1000 %
1000 %
ASTM D4325
Thermal Properties Metric English Comments
Thermal Conductivity 7.28 W/m-K
50.4 BTU-in/hr-ft²-°F
ASTM D1518
Maximum Service Temperature, Air 90.0 °C
194 °F
Continuous
130 °C
266 °F
Emergency Overload
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
ASTM D1000
Dielectric Strength 28.3 kV/mm
720 kV/in
After 96 hrs @ 96% RH; ASTM D4325
31.5 kV/mm
800 kV/in
Standard Conditioning; ASTM D4325
Descriptive Properties Value Comments
Appearance Black