DuPont Performance Polymers Minlon® 22C BK086 Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer DuPont Performance Polymers
Trade Name Minlon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Minlon® 22C BK086 Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C BK086 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 72.0 MPa
10400 psi
50%RH; ISO 527-1/-2
120 MPa
17400 psi
DAM; ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
DAM; ISO 527-1/-2
4.0 %
4.0 %
50%RH; ISO 527-1/-2
Tensile Modulus 5.00 GPa
725 ksi
50%RH; ISO 527-1/-2
7.50 GPa
1090 ksi
DAM; ISO 527-1/-2
Flexural Modulus 7.00 GPa
1020 ksi
DAM; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
DAM; ISO 180/1A
3.40 kJ/m²

@Temperature -40.0 °C
1.62 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 180/1A
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 41.0 µm/m-°C
22.8 µin/in-°F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 62.0 µm/m-°C
34.4 µin/in-°F
DAM; ISO 11359-1/-2
Melting Point 263 °C
505 °F
DAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 255 °C
491 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
DAM; ISO 75-1/-2
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
DAM; IEC 60695-11-10
Flame Spread 23 mm/min

@Thickness 1.00 mm
0.91 in/min

@Thickness 0.0394 in
SE/B; ISO 3795 (FMVSS 302)
Electrical Properties Metric English Comments
Comparative Tracking Index 475 V
475 V
DAM; IEC 60112
Descriptive Properties Value Comments
Part Marking Code >PA66-(MD+GF)38<
ISO 11469
Regional Availability Asia Pacific
North America
South and Central America
Resin Identification PA66-(MD+GF)38
Special Characteristics Heat stabilised or stable to heat