EMS-Grivory Grivory® R 50 H NZ PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® R 50 H NZ PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon R 50 H NZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon R 50 H NZ has the following important properties: Very high melt strengthHigh impact resistance even at low temperaturesVery good weld line strengthProcessable on conventional as well as on 3 D-machinesSuitable for sequential blow molding process in combination with flexible grades Grilon R 50 H NZ is used typically for automotive applications such are air ducts for turbo-chargers, air ducts, oil filler pipes, fuel and oil containers.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 30.0 MPa
4350 psi
conditioned; ISO 2039-1
90.0 MPa
13100 psi
dry; ISO 2039-1
Tensile Stress 25.0 MPa

@Strain 50.0 %
3630 psi

@Strain 50.0 %
conditioned; ISO 527-1/-2
Tensile Strength, Yield 50.0 MPa
7250 psi
dry; ISO 527-1/-2
50.0 MPa
7250 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
dry; ISO 527-1/-2
5.0 %
5.0 %
dry; ISO 527-1/-2
Tensile Modulus 0.600 GPa
87.0 ksi
conditioned; ISO 527-1/-2
1.80 GPa
261 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 9.50 J/cm²
45.2 ft-lb/in²
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
2.50 J/cm²

@Temperature 30.0 °C
11.9 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
2.50 J/cm²

@Temperature 30.0 °C
11.9 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 130 µm/m-°C
72.2 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°C
77.8 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
180 °C
356 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Comparative Tracking Index 475 V
475 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Cooling and climate control
Hydraulic systems
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Extrusion - blow molding
Other Extrusion
Special Characteristics High impact or impact modified
Improved heat resistance