Solvay TECHNYL® C 218 V40 PA6, 40% glass fiber, Eh 50

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 218 V40 PA6, 40% glass fiber, Eh 50.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL C 218 V40 is a polyamide 6 with 40% of glass fiber and with thermal stability.Colors: it is marketed in the black color and natural.Available in: Latin AmericaMain Properties: ? Good thermal resistance, ?Excellent dimensional stability, Good impact resistance. Applications: TECHNYL C 218 V40 was developed for applications on parts where good mechanical properties as impact resistance, superficial aspect and dimensional stability are required.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 140 MPa
20300 psi
ISO R 527
Elongation at Break 3.5 %
3.5 %
ISO R 527
Tensile Modulus 7.30 GPa
1060 ksi
ISO R 527
Izod Impact, Notched (ISO) 34.0 kJ/m²
16.2 ft-lb/in²
ISO 180
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
ISO 179
Charpy Impact, Notched 3.40 J/cm²
16.2 ft-lb/in²
ISO 179
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
CEI 93
Dielectric Constant 4.5
4.5
CEI 250
Dielectric Strength 22.0 kV/mm
559 kV/in
CEI 93
Dissipation Factor 0.0090
0.0090
CEI 250
Comparative Tracking Index 475 V
475 V
CEI 112