Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Comshield® 220 ABS, Electrically Conductive - Carbon Black Filled

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
Manufacturer A. Schulman ComAlloy
Trade Name Comshield®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Comshield® 220 ABS, Electrically Conductive - Carbon Black Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Ultimate 43.0 MPa
6240 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 57.0 MPa
8270 psi
ASTM D790
Flexural Modulus 4.00 GPa
580 ksi
ASTM D790
Izod Impact, Unnotched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 100 - 1000 ohm-cm