Electrical Properties Metric English Comments
Electrical Resistivity 0.200 - 1000 ohm-cm
0.200 - 1000 ohm-cm
Average value: 257 ohm-cm Grade Count:4
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va..
Electrical Resistivity 0.200 - 1.00e+16 ohm-cm
0.200 - 1.00e+16 ohm-cm
Average value: 1.73e+15 ohm-cm Grade Count:175
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Electrical Resistivity 0.200 ohm-cm
0.200 ohm-cm
Through-Plane
GrafTech eGRAF® SPREADERSHIELD™ SS1500 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Copyright © lookpolymers.com All Rights Reserved