Melt Temperature |
180 - 246 °C |
356 - 475 °F |
Average value: 219 °C Grade Count:7 |
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
Melt Temperature |
232 - 246 °C |
450 - 475 °F |
|
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp.. |
Melt Temperature |
204 - 246 °C |
400 - 475 °F |
|
RTP Company EMI 660.5 Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
|
Melt Temperature |
204 - 246 °C |
400 - 475 °F |
|
RTP Company EMI 660.5 FR A Acrylonitrile Butadiene Styrene (ABS) Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - Flame Retardant
|
Melt Temperature |
204 - 246 °C |
400 - 475 °F |
|
RTP Company EMI 660.6 Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
|
Melt Temperature |
204 - 246 °C |
400 - 475 °F |
|
RTP Company EMI 661 FR A Acrylonitrile Butadiene Styrene (ABS); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
|
Melt Temperature |
204 - 246 °C |
400 - 475 °F |
|
RTP Company EMI 661 FR Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
|
Melt Temperature |
204 - 246 °C |
400 - 475 °F |
|
RTP Company EMI 662 Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
|
Melt Temperature |
204 - 246 °C |
400 - 475 °F |
|
RTP Company EMI 662 FR A Acrylonitrile Butadiene Styrene (ABS); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
|
Melt Temperature |
221 - 246 °C |
430 - 475 °F |
|
RTP Company PermaStat® 301 FR Polycarbonate (PC), ESD Protection - Permanently Anti-static - Glass Fiber - Flame Retardant
|
Melt Temperature |
218 - 246 °C |
425 - 475 °F |
|
RTP Company RTP 1503-72D Polyether-Ester Block Copolymer (TEEE / COPE), Glass Fiber
|
Melt Temperature |
204 - 246 °C |
400 - 475 °F |
|
RTP Company EMI 660.75 Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
|
Melt Temperature |
204 - 246 °C |
400 - 475 °F |
|
RTP Company EMI 662 FR Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
|
Melt Temperature |
204 - 246 °C |
400 - 475 °F |
|
RTP Company EMI 663 Acrylonitrile Butadiene Styrene (ABS) Stainless Steel Fiber - EMI/RFI Shielding
|
Melt Temperature |
204 - 246 °C |
400 - 475 °F |
|
Clariant ABS4500 ABS, High Impact
Data provided by Clariant Masterbatches |
Melt Temperature |
232 - 246 °C |
450 - 475 °F |
|
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose
Data provided by Clariant Masterbatches |
Melt Temperature |
188 - 246 °C |
370 - 475 °F |
Average value: 223 °C Grade Count:54 |
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
Melt Temperature |
218 - 246 °C |
425 - 475 °F |
|
RTP Company RTP 2099 x 121825 E Biobased Polyamide (PA) Permanently Anti-static - ESD Protection - 31% Bio-Content
|