Covestro Desmopan® DP 2586A Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® DP 2586A Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extrusion- and injection molding gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentBeadsApplicationBlown filmsPreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Melt
1.19 g/cc
0.0430 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
3s; ISO 868
Hardness, Shore D 38
38
15s; ISO 868
Abrasion 32
32
mm³; ISO 4649
Compression Set 23 %

@Temperature 23.0 °C
23 %

@Temperature 73.4 °F
ISO 815
45 %

@Temperature 70.0 °C
45 %

@Temperature 158 °F
ISO 815
Thermal Properties Metric English Comments
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Thermal Conductivity 0.138 W/m-K
0.958 BTU-in/hr-ft²-°F
Melt
Processing Properties Metric English Comments
Melt Temperature 210 - 230 °C
410 - 446 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Ejection Temperature 50.0 °C
122 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America
Eff. thermal diffusivity (m²/s) 8.04E-08