Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
PolyOne OnFlex™ S HF 50A-3S1981 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
PolyOne OnFlex™ S HF 60A-3S1982 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
PolyOne OnFlex™ S HF 70A-3S1984 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
PolyOne OnFlex™ S HF 80A-3S1986 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
PolyOne OnFlex™ S HF 90A-3S1988 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Melt Temperature | 170 - 180 °C | 338 - 356 °F | |
PolyOne Geon™ Vinyl Flexible R1480E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
Lotte Chemical Titan TITANLENE® LDF268GG Low density polyethylene LDF268GG is a low density polyethylene resin for film extrusion. LDF268GG has medium slip and anti-block additives. LDF268GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
Lucobit Lucofin® 1414-t1 Polyolefin TPO Granules, Silk Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
Lotte Chemical Titan TITANLENE® LDF200GG Low density polyethylene LDF200GG is a low density polyethylene resin for film extrusion. LDF200GG has medium slip and anti-block additives. LDF200GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
Lotte Chemical Titan TITANLENE® LDF200YZ Low density polyethylene LDF200YZ is a low density polyethylene resin for film extrusion. LDF200YZ has no slip and anti-block additives. LDF200YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
Lotte Chemical Titan TITANLENE® LDF260GG Low density polyethylene LDF260GG is a low density polyethylene resin for film extrusion. LDF260GG has medium slip and anti-block additives. LDF260GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
Lucobit Lucofin® 1413-t1 Polyolefin TPO Granules, Dark Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Melt Temperature | 140 - 180 °C | 284 - 356 °F | Injection Molding |
Stellarchem MP-835B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 150 - 180 °C | 302 - 356 °F | Extrusion |
Stellarchem SV-B40D TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Melt Temperature | 150 - 180 °C | 302 - 356 °F | Extrusion |
Stellarchem SV-B65E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Melt Temperature | 150 - 180 °C | 302 - 356 °F | Extrusion |
Stellarchem SV-B70E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Melt Temperature | 150 - 180 °C | 302 - 356 °F | Extrusion |
Stellarchem SV-B75E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Melt Temperature | 150 - 180 °C | 302 - 356 °F | Extrusion |
Stellarchem SV-B87E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Melt Temperature | 150 - 180 °C | 302 - 356 °F | |
Borealis FA6224 Low Density Polyethylene FA6224 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed for the production of thin blown f.. |
|||
Melt Temperature | 150 - 180 °C | 302 - 356 °F | |
Borealis FA7220 Low Density Polyethylene FA7220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for production of blown film or cast film with good optical properties. When cast on a polish.. |
|||
Melt Temperature | 140 - 180 °C | 284 - 356 °F | |
Borealis FA7224 Low Density Polyethylene FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG.. |
|||
Melt Temperature | 140 - 180 °C | 284 - 356 °F | |
Borealis FA7229 Low Density Polyethylene FA7229 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant and Cling additive. Applications: food wrap film, lamination films, blending, and other blown cling film.Information pr.. |
|||
Melt Temperature | 140 - 180 °C | 284 - 356 °F | |
Borealis LE0563 Polyethylene Compound, Thermoplastic, Semiconductive LE0563 is a thermoplastic semi conductive compound specifically designed for medium- and high voltage cable systems requiring improved grounding. It may be used either as a complete jacket or as a t.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
Tisan TISAKRIL® 15% Glass Fiber Reinforced ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
Tisan TISAKRIL® Flame Retardant (V0) ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
Tisan TISAKRIL® UNR ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
Tisan TISREN® Flame Retardant (V0) Polystyrene TISREN has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimensio.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
Lucobit Lucofin® 1412-t1 Polyolefin TPO Granules, Light Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
Tisan TISAKRIL® 30% Glass Fiber Reinforced ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Melt Temperature | 160 - 180 °C | 320 - 356 °F | |
SABIC HP2022 Series Low Density Polyethylene for Blown Film Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:.. |