Stellarchem SV-B40D TPV Compound

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Stellarchem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stellarchem SV-B40D TPV Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on conventional thermoplastics equipment for extrusion or blow molding, provides the performance of vulcanized rubber with the advantage of low cost thermoplastic processing. It's a soft, EPDM/PP based, completely recyclable & colorable elastomer material. It's formulated to overmold to PP thermoplastics in normal dual injection & extrusion processing.Information provided by Stellarchem Polymer & Industrial
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Particle Mesh Size 80 - 150 Mesh
80 - 150 Mesh
Melt Flow 78 g/10 min

@Load 10.0 kg,
Temperature 230 °C
78 g/10 min

@Load 22.0 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
ASTM D2240
Tensile Strength, Ultimate 17.3 MPa
2500 psi
ASTM D412
Elongation at Break 770 %
770 %
ASTM D412
100% Modulus 0.0980 GPa
14.2 ksi
ASTM D412
Tear Strength 95.1 kN/m
543 pli
ASTM D412
Processing Properties Metric English Comments
Processing Temperature 160 - 170 °C
320 - 338 °F
Metering Temperature, Extrusion
Rear Barrel Temperature 150 - 160 °C
302 - 320 °F
Extrusion
160 - 190 °C
320 - 374 °F
Injection Molding
Middle Barrel Temperature 155 - 165 °C
311 - 329 °F
Transition, Extrusion
170 - 190 °C
338 - 374 °F
Injection Molding
Front Barrel Temperature 170 - 180 °C
338 - 356 °F
Extrusion
180 - 200 °C
356 - 392 °F
Injection Molding
Nozzle Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
Die Temperature 170 - 180 °C
338 - 356 °F
Extrusion
Melt Temperature 150 - 180 °C
302 - 356 °F
Extrusion
160 - 200 °C
320 - 392 °F
Injection Molding
Mold Temperature 25.0 - 40.0 °C
77.0 - 104 °F
Injection Molding
Injection Pressure 5.00 - 40.0 MPa
725 - 5800 psi
Injection Molding
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Injection Molding
Screw Speed 60 - 100 rpm
60 - 100 rpm
Extrusion
100 - 200 rpm
100 - 200 rpm
Injection Molding