Material Notes:
LE0563 is a thermoplastic semi conductive compound specifically designed for medium- and high voltage cable systems requiring improved grounding. It may be used either as a complete jacket or as a thin layer extruded on top of the jacket. This compounds permits easy diagnostic testing of the cable to ensure jacket conformity, allowing confirmation of fault-free cable before and after installation. It provides superior environmental stress crack resistance and good electrical conductivity. Due to the semi conductive properties, it will also provide added protection against lightning strikes. Specifications: BS 6622; IEC 60502; and IEC 60840.Information provided by Borealis AG
Physical Properties Metric English Comments
Water Absorption 0.040 %
0.040 %
Karl Fischer-titration
Environmental Stress Crack Resistance >= 2.0 hour

@Temperature 50.0 °C
>= 2.0 hour

@Temperature 122 °F
Igepal 10%/Seawater;F0
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
1s; ISO 868
Tensile Strength at Break 3.125 MPa
453.2 psi
after aging 240h, 100°C;IEC 60811-1-2
12.5 MPa
1810 psi
25mm/min; ISO 527
Elongation at Break 400 %
400 %
25mm/min; ISO 527
Electrical Properties Metric English Comments
Volume Resistivity <= 50 ohm-cm

@Temperature 23.0 °C
<= 50 ohm-cm

@Temperature 73.4 °F
ISO 3915
<= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ISO 3915
Processing Properties Metric English Comments
Zone 1 130 °C
266 °F
Zone 2 140 °C
284 °F
Zone 3 150 °C
302 °F
Zone 4 180 °C
356 °F
Die Temperature 180 °C
356 °F
Melt Temperature 140 - 180 °C
284 - 356 °F