Material Notes:
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, completely recyclable, colorable & non-hygroscopic thermoplastics elastomer material.Information provided by Stellarchem Polymer & Industrial
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
Melt Flow 47.8 g/10 min
47.8 g/10 min
JIS K7210
Mechanical Properties Metric English Comments
Hardness, Shore A 36
36
JIS K6301
Tensile Strength, Ultimate 1.27 MPa
185 psi
JIS K6301
Elongation at Break 623 %
623 %
JIS K6301
100% Modulus 0.00490 GPa
0.711 ksi
JIS K6301
300% Modulus 0.000294 GPa
0.0427 ksi
JIS K6301
Tear Strength 1.08 kN/m
6.16 pli
JIS K6301-B
Processing Properties Metric English Comments
Rear Barrel Temperature 140 - 160 °C
284 - 320 °F
Injection Molding
Middle Barrel Temperature 150 - 170 °C
302 - 338 °F
Injection Molding
Front Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
Nozzle Temperature 170 - 180 °C
338 - 356 °F
Injection Molding
Melt Temperature 140 - 180 °C
284 - 356 °F
Injection Molding
Mold Temperature 25.0 - 40.0 °C
77.0 - 104 °F
Injection Molding
Injection Pressure 5.00 - 40.0 MPa
725 - 5800 psi
Injection Molding
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Injection Molding
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding