Material Notes:
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on conventional thermoplastics equipment for injection molding or extrusion, provides the performance of vulcanized rubber with the advantage of low cost thermoplastic processing. It's a soft, EPDM/PP based, completely recyclable & colorable elastomer material. It's formulated to overmold to PP thermoplastics in normal dual injection & extrusion processing.Information provided by Stellarchem Polymer & Industrial
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Particle Mesh Size 80 - 150 Mesh
80 - 150 Mesh
Melt Flow 22 g/10 min

@Load 10.0 kg,
Temperature 230 °C
22 g/10 min

@Load 22.0 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength, Ultimate 8.83 MPa
1280 psi
ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
100% Modulus 0.04116 GPa
5.970 ksi
ASTM D412
Tear Strength 38.2 kN/m
218 pli
ASTM D412
Compression Set 43 %

@Temperature 70.0 °C,
Time 79200 sec
43 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Processing Properties Metric English Comments
Processing Temperature 160 - 170 °C
320 - 338 °F
Metering Temperature, Extrusion
Rear Barrel Temperature 150 - 160 °C
302 - 320 °F
Extrusion
160 - 190 °C
320 - 374 °F
Injection Molding
Middle Barrel Temperature 155 - 165 °C
311 - 329 °F
Transition, Extrusion
170 - 190 °C
338 - 374 °F
Injection Molding
Front Barrel Temperature 170 - 180 °C
338 - 356 °F
Extrusion
180 - 200 °C
356 - 392 °F
Injection Molding
Nozzle Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
Die Temperature 170 - 180 °C
338 - 356 °F
Extrusion
Melt Temperature 150 - 180 °C
302 - 356 °F
Extrusion
160 - 200 °C
320 - 392 °F
Injection Molding
Mold Temperature 25.0 - 40.0 °C
77.0 - 104 °F
Injection Molding
Injection Pressure 5.00 - 40.0 MPa
725 - 5800 psi
Injection Molding
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Injection Molding
Screw Speed 60 - 100 rpm
60 - 100 rpm
Extrusion
100 - 200 rpm
100 - 200 rpm
Injection Molding