DuPont Performance Polymers Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 40% Glass Fiber Reinforced
Manufacturer DuPont Performance Polymers
Trade Name Zytel® HTN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® HTN51G35NOX BK083 is a 35% glass reinforced high performance polyamide resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution. It is also a PPA resin.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
DAM; ISO 1183
Filler Content 35 %
35 %
DAM
Mechanical Properties Metric English Comments
Tensile Strength at Break 215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 2.3 %

@Temperature 23.0 °C
2.3 %

@Temperature 73.4 °F
DAM; ISO 527
Tensile Modulus 11.5 GPa

@Temperature 23.0 °C
1670 ksi

@Temperature 73.4 °F
DAM; ISO 527
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 264 °C
507 °F
DAM; ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 325 °C
617 °F
DAM; Optimum
320 - 330 °C
608 - 626 °F
DAM
Mold Temperature 150 °C
302 °F
DAM; optimum
140 - 160 °C
284 - 320 °F
DAM
Drying Temperature 100 °C
212 °F
DAM
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
Moisture Content <= 0.10 %
<= 0.10 %
DAM
Descriptive Properties Value Comments
Appearance Black Color
DAM
Filler Glass Reinforced
DAM
Forms Pellets
DAM
Generic Polyphthalamide (PPA)
DAM
Material Status Preliminary Data
DAM
Part Marking Code >PA6T/XT-GF35<
ISO 11469; DAM
>PPA-GF35<
SAE J1344; DAM
Processing Method Injection Molding
DAM
Product Category Glass Reinforced Resins
DAM
Region Available - Global Yes
DAM
Resin Identification PA6T/XT-IGF35
ISO 1043; DAM
RoHS Compliance Contact Manufacturer
DAM