Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420J Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 40% Glass Fiber Reinforced
Manufacturer DuPont Performance Polymers
Trade Name Zytel® HTN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420J Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
35% Glass Reinforced PPA High Performance Polyamide with Improved Surface Appearance Zytel HTN51G35HSLR BK420J is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance and surface appearaInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 215 MPa
31200 psi
DAM; ISO 527-1/-2
Elongation at Break 2.6 %
2.6 %
DAM; ISO 527-1/-2
Tensile Modulus 11.5 GPa
1670 ksi
DAM; ISO 527-1/-2
Flexural Modulus 10.3 GPa
1490 ksi
DAM; ISO 178
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 264 °C
507 °F
DAM; ISO 75-1/-2
Descriptive Properties Value Comments
Part Marking Code >PA6T/XT-GF35<
ISO 11469
>PPA-GF35<
SAE J1344
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Special Characteristics Heat stabilised or stable to heat