Processing Properties Metric English Comments
Drying Temperature 93.3 - 107 °C
200 - 225 °F
Polymer Resources PPX/NY G10 PPO/Nylon 66 Alloy , 10% Glass Reinforced
Polyphenylene Oxide/Nylon 66 Alloy , 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Drying Temperature 93.3 - 107 °C
200 - 225 °F
Polymer Resources PPX/NY G20 PPO/Nylon 66 Alloy , 20% Glass Reinforced
Polyphenylene Oxide/Nylon 66 Alloy , 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Drying Temperature 93.3 - 107 °C
200 - 225 °F
Polymer Resources PPX/NY G30 PPO/Nylon 66 Alloy , 30% Glass Reinforced
Polyphenylene Oxide/Nylon 66 Alloy , 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Drying Temperature 93.3 - 107 °C
200 - 225 °F
Polymer Resources PPX/NY GP1 PPO/Nylon 66 Alloy
Polyphenylene Oxide/Nylon 66 Alloy , General PurposeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Drying Temperature 93.3 - 107 °C
200 - 225 °F
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat
Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Drying Temperature 93.3 - 107 °C
200 - 225 °F
PolyOne Edgetek® NY-20CF/000 BLACK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Drying Temperature 93.3 - 107 °C
200 - 225 °F
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated  (discont
Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Drying Temperature 82.2 - 107 °C
180 - 225 °F
PolyOne Lubri-Tech™ PS-30CF/10T 2S Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced, PTFE/Silicone Lubricated
Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Drying Temperature 93.3 - 107 °C
200 - 225 °F
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 75.0 - 107 °C
167 - 225 °F
Average value: 86.2 °C Grade Count:67
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Drying Temperature 75.0 - 107 °C
167 - 225 °F
Average value: 88.7 °C Grade Count:39
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Drying Temperature 75.0 - 107 °C
167 - 225 °F
Average value: 85.1 °C Grade Count:16
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Drying Temperature 75.0 - 107 °C
167 - 225 °F
Average value: 87.6 °C Grade Count:43
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Drying Temperature 75.0 - 107 °C
167 - 225 °F
Average value: 90.1 °C Grade Count:12
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Drying Temperature 75.0 - 107 °C
167 - 225 °F
Average value: 85.8 °C Grade Count:6
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
Drying Temperature 79.4 - 107 °C
175 - 225 °F
Average value: 82.3 °C Grade Count:8
Overview of materials for Nylon 612 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app..
Drying Temperature 79.4 - 107 °C
175 - 225 °F
Average value: 83.6 °C Grade Count:5
Overview of materials for Nylon 612, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of..
Drying Temperature 93.0 - 107 °C
199 - 225 °F
PolyOne Lubri-Tech™ NL-000/40T Nylon 6/12 - 40% PTFE  (discontinued **)
Data provided by PolyOne.
Drying Temperature 93.0 - 107 °C
199 - 225 °F
PolyOne Lubri-Tech™ NL-10GF/15TF Nylon 6/12 - 10% Glass Fiber - 15% PTFE Flock  (discontinued **)
Data provided by PolyOne.
Drying Temperature 93.0 - 107 °C
199 - 225 °F
PolyOne Lubri-Tech™ NL-15KV/05M Nylon 6/12 - 15% Kevlar Fiber - 5% MoS2  (discontinued **)
Data provided by PolyOne.
Drying Temperature 79.4 - 107 °C
175 - 225 °F
Average value: 83.9 °C Grade Count:21
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values..
Drying Temperature 93.3 - 107 °C
200 - 225 °F
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 93.3 - 107 °C
200 - 225 °F
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 93.3 - 107 °C
200 - 225 °F
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 93.3 - 107 °C
200 - 225 °F
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 80.0 - 107 °C
176 - 225 °F
Average value: 100 °C Grade Count:13
Overview of materials for Polyphthalamide (PPA), Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a..
Drying Temperature 80.0 - 107 °C
176 - 225 °F
Average value: 99.0 °C Grade Count:18
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi..
Copyright © lookpolymers.com All Rights Reserved