PolyOne Stat-Tech™ NN-30CF/000 Black Polyamide 66 (Nylon 66)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer PolyOne Corporation
Trade Name Stat-Tech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Stat-Tech™ NN-30CF/000 Black Polyamide 66 (Nylon 66).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber for low to high levels of conductivity depending upon application requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 228 MPa
33100 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 331 MPa
48000 psi
ASTM D790
Flexural Modulus 17.2 GPa
2490 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Electrical Properties Metric English Comments
Volume Resistivity 1.0 - 1000 ohm-cm
1.0 - 1000 ohm-cm
ASTM D257
Surface Resistance 1.0 - 1000 ohm
1.0 - 1000 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 282 - 310 °C
540 - 590 °F
Mold Temperature 93.3 - 107 °C
200 - 225 °F
Drying Temperature 71.1 - 82.2 °C
160 - 180 °F
Descriptive Properties Value Comments
Features Good Chemical Resistance
High Stiffness
Semi Crystalline
Filler / Reinforcement Carbon Fiber Reinforcement, 30% Filler by Weight
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Aerospace Applications
Business Equipment
Computer Components
Connectors
Electrical/Electronic Applications