Polymer Property : Drying Temperature = 170 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 71.1 - 76.7 °C
160 - 170 °F
PolyOne LubriOne™ GF-1010 40 MS 2 HS Black 37 Polyamide 6 (Nylon 6)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Drying Temperature 71.1 - 76.7 °C
160 - 170 °F
PolyOne LubriOne™ NL-30GF/15T Black Polyamide 612 (Nylon 612)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Drying Temperature 71.1 - 76.7 °C
160 - 170 °F
PolyOne LubriOne™ NN-000/15T Polyamide 66 (Nylon 66)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Drying Temperature 71.1 - 76.7 °C
160 - 170 °F
4 hours
Ineos ABS Lustran® 451 ABS, Injection Molding Grade
Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss.
Drying Temperature 71.1 - 76.7 °C
160 - 170 °F
4 hours
Ineos ABS Lustran® ABS 349
Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives.