Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers Tekaster® F615GM , 40% GF/MF Reinforced PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKASTER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers Tekaster® F615GM , 40% GF/MF Reinforced PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% GF/MF Reinforced, Low warpageInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 98.0 MPa
14200 psi
ASTM D638
Elongation at Break 2.3 %
2.3 %
ASTM D638
Flexural Yield Strength 150 MPa
21800 psi
ASTM D790
Flexural Modulus 9.60 GPa
1390 ksi
ASTM D790
Izod Impact, Notched 0.680 J/cm
1.27 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
464 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 270 - 300 °C
518 - 572 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Users viewing this material also viewed the following: