Processing Properties Metric English Comments
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced
Polycarbonate, 10% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G10-[color]-1 Polycarbonate, 10% Glass Reinforced with Mold Release
Polycarbonate, 10% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G10-IM Polycarbonate, 10% Glass Reinforced, Impact Modified
Polycarbonate, 10% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G20 Polycarbonate, 20% Glass Reinforced
Polycarbonate, 20% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G20-[color]-1 Polycarbonate, 20% Glass Reinforced with Mold Release
Polycarbonate, 20% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G20-[color]-WS Polycarbonate, 20% Glass Reinforced
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced
Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G40 Polycarbonate, 40% Glass Reinforced
Polycarbonate, 40% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G40-[color]-1 Polycarbonate, 40% Glass Reinforced with Mold Release
Polycarbonate, 40% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR1-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-G30-[color]-1 Polycarbonate, 30% Glass Reinforced with Mold Release
Polycarbonate, 30% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant
Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
LTL Color Compounds ColorFast® PCGF120 Polycarbonate, 20% Glass-Filled
20% glass-filled grade, good balance of impact and mechanical propertiesAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
LTL Color Compounds ColorFast® PCGF130 Polycarbonate, 30% Glass-Filled
30% glass-filled grade polycarbonateAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Polymer Resources PCSF-FRG20 Polycarbonate, 20% Glass Reinforced Structural Foam Grade
Polycarbonate, 20% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con..
Front Barrel Temperature 316 - 338 °C
600 - 640 °F
Celanese FORTRON® 1140 E7 Polyphenylene Sulfide (PPS)
Description: Fortron 1140E7 is an inherently flame-retardant grade exhibiting extremely low flash and fast cycle times. It has excellent electrical properties, high hardness and stiffness. This grad..