Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stability, chemical resistance and ductility. This resin has a high heat deflection temperature and a high flexural modulus, with greater tensile elongation than untoughened glass-reinforced PPA.Features: Good Chemical Resistance; Good Dimensional Stability; Heat Stabilized; High Heat Resistance; Impact ModifiedUses: Appliance Components; Appliances; Automotive Applications; Automotive Electronics; Automotive Under the Hood; Bearings; Connectors; Fuel Lines; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal ReplacementInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D4000 PA123 G25; ASTM D4000 PPA0111 G25 KD160 KN075 LD002 PN080 YI250; ASTM D6779 PA123G25; ISO 1874 PA6T/6I/66-HI, MH, 12-080, GF25Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Dry; ISO 1183
Filler Content 25 %
25 %
Glass Fiber
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
Dry
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Dry; ASTM D955
Mechanical Properties Metric English Comments
Flexural Yield Strength 200 MPa
29000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.00 J/cm
15.0 ft-lb/in
ASTM D256
Dart Drop, Total Energy 9.36 J
6.90 ft-lb
Instrumented; ASTM D3763
Thermal Properties Metric English Comments
Melting Point 311 °C
592 °F
Peak; Dry; ASTM D3418
311 °C
592 °F
Dry; ISO 11357-3
Processing Properties Metric English Comments
Processing Temperature 79.4 °C
175 °F
Hopper
Rear Barrel Temperature 304 - 318 °C
579 - 604 °F
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Melt Temperature 321 - 343 °C
610 - 649 °F
Mold Temperature 135 °C
275 °F
Drying Temperature 121 °C

@Time 14400 sec
250 °F

@Time 4.00 hour
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Impact Modifier
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black
Form Pellets
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant