Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-GP1-[color]H Nylon, General Purpose, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-200N Nylon 6 with Nucleating Agent Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-600 Medium Viscosity Extrusion Grade Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6 Total Extractables < 1.5.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-IM1 Nylon 6, Impact Modified Nylon 6, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-IM1-[color]-H Nylon 6, Impact Modified, Heat Stabilized Nylon 6, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegis™ H73MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H73MP is a lubricated nucleated low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR .. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegis™ H85ZP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H85ZP is a medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H100QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100QP is a lubricated medium viscosity, Nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500 as well as EU Directiv.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well .. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H73QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73QP is a lubricated low viscosity, nylon 6 extrusion grade homopolymer for cast coextrusion. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H85QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H85QP is a lubricated, medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 a.. |
|||
Middle Barrel Temperature | 241 - 254 °C | 466 - 489 °F | Injection Molding |
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)... |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
LTL Color Compounds ColorFast® FRPBT200 PBT, Flame Retarded V-0 rated, unfilled PBTAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
LTL Color Compounds ColorFast® FRPBT210 PBT, Flame Retarded, Impact Modified V-0 rated, impact modified unfilled PBTAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 243 - 254 °C | 470 - 490 °F | |
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc. |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 241 - 254 °C | 465 - 490 °F | |
Calsak CS-72 General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc. |