Processing Properties Metric English Comments
Middle Barrel Temperature 227 - 238 °C
440 - 460 °F
Polymer Resources NY6/12-GP1 General Purpose Nylon 612
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Middle Barrel Temperature >= 227 °C
>= 440 °F
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
Middle Barrel Temperature 227 - 271 °C
440 - 520 °F
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Middle Barrel Temperature 227 - 271 °C
440 - 520 °F
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Middle Barrel Temperature 227 - 271 °C
440 - 520 °F
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 185F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Middle Barrel Temperature >= 227 °C
>= 440 °F
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade
Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc..
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
PTS Trimid® N6-200L Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
PTS Trimid® N6-200N Nylon 6 with Nucleating Agent
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
PTS Trimid® N6-600 Medium Viscosity Extrusion Grade Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6
Total Extractables < 1.5.Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
PTS Trimid® N6-G13L 13% GFR Lubricated Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
PTS Trimid® N6-G15HL 15% GFR Heat Stabilized Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
PTS Trimid® N6-G15L 15% GFR Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
PTS Trimid® N6-G30L 30% GFR Lubricated Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
PTS Trimid® N6-G33L 33% GFR Lubricated Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 227 - 243 °C
440 - 470 °F
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black
Middle Barrel Temperature 227 °C
441 °F
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro..
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose
Data provided by Clariant Masterbatches
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Middle Barrel Temperature 227 - 271 °C
440 - 520 °F
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 227 - 271 °C
440 - 520 °F
Polymer Resources PPX-FR2 Modified PPO, UL 94 V-1 with HDT of 210 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 227 - 271 °C
440 - 520 °F
Polymer Resources PPX-FR4 Modified PPO, UL 94 V-1 with HDT of 185 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.