Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegis™ H73MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H73MP is a lubricated nucleated low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR .. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegis™ H85MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H85MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 C.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegis™ H85ZP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H85ZP is a medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegis™ H135KQP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135KQP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to applicable FDA requirements, including 21 CFR 177.1500 for N6 an.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegis™ H205QP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H205QP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500. It possesses the combination.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 .. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H100QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100QP is a lubricated medium viscosity, Nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500 as well as EU Directiv.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well .. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H135QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135QP is a lubricated high viscosity, N6, film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements including, 21 CFR 177.1500 as well as EU Direct.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H155ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H155ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well a.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H73QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73QP is a lubricated low viscosity, nylon 6 extrusion grade homopolymer for cast coextrusion. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H85QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H85QP is a lubricated, medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 a.. |
|||
Middle Barrel Temperature | 241 - 254 °C | 466 - 489 °F | Injection Molding |
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)... |
|||
Middle Barrel Temperature | 241 - 254 °C | 466 - 489 °F | Injection Molding |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |