PTS Trimid® N6-600 Medium Viscosity Extrusion Grade Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer Polymer Technology & Services, LLC (PTS)
Trade Name Trimid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PTS Trimid® N6-600 Medium Viscosity Extrusion Grade Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 82.7 MPa
12000 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Yield Strength 102 MPa
14800 psi
ASTM D790
Izod Impact, Notched 0.370 J/cm

@Thickness 3.17 mm
0.693 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648
Flammability, UL94 V-2

@Thickness 3.17 mm
V-2

@Thickness 0.125 in
Processing Properties Metric English Comments
Rear Barrel Temperature <= 216 °C
<= 420 °F
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
Front Barrel Temperature 238 - 266 °C
460 - 510 °F
Nozzle Temperature 238 - 266 °C
460 - 510 °F
Melt Temperature 232 - 271 °C
450 - 520 °F
Mold Temperature 21.1 - 93.3 °C
70.0 - 200 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 3 - 4 hour
3 - 4 hour
Injection Pressure 82.7 - 172 MPa
12000 - 25000 psi
Back Pressure 0.000 - 0.345 MPa
0.000 - 50.0 psi
Screw Speed 40 - 80 rpm
40 - 80 rpm