Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-GP1-[color]H Nylon, General Purpose, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Middle Barrel Temperature | 243 - 254 °C | 470 - 490 °F | |
Polymer Resources PC/ASA-GP2 Polycarbonate/ASA Alloy Acrylonitrile Styrene Acrylate + PolycarbonatePreliminary DataProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-200N Nylon 6 with Nucleating Agent Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-600 Medium Viscosity Extrusion Grade Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6 Total Extractables < 1.5.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-G13L 13% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-G15HL 15% GFR Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-IM1 Nylon 6, Impact Modified Nylon 6, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-IM1-[color]-H Nylon 6, Impact Modified, Heat Stabilized Nylon 6, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
LTL Color Compounds ColorFast® FRPBT200 PBT, Flame Retarded V-0 rated, unfilled PBTAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
LTL Color Compounds ColorFast® FRPBT210 PBT, Flame Retarded, Impact Modified V-0 rated, impact modified unfilled PBTAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
LTL Color Compounds ColorFast® PBT100 PBT General purpose injection molding grade unfilled PBT with lubeAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 243 - 254 °C | 470 - 490 °F | |
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc. |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 241 - 254 °C | 465 - 490 °F | |
Calsak CS-72L General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc. |